GOTECH Creep Tester (GT-7049-DH)

Description

PRINCIPLE

The creep tester is used to measure the strain of a material under long-term loading. Tests can be conducted at various temperatures to simulate the conditions the material may encounter in real-world applications.

Suitable for a variety of industries:

It is suitable for industries such as materials science, civil engineering, aerospace, academic research, and general industrial manufacturing.

Stress relaxation:

When a constant strain is applied to rubber, the force that maintains the strain is not constant; it gradually decreases over time.

Creep:

When a constant stress is applied to rubber, the deformation that maintains the stress is not constant; it gradually increases over time.

Static creep:

The phenomenon that the displacement of a rubber elastic element gradually increases over time under a constant static load.

Static stress relaxation:

The phenomenon that the force exerted by a rubber elastic element gradually decreases over time under constant deformation.

Compression stress relaxation:

The phenomenon that the compressive force gradually decreases over time after a specimen is subjected to constant compression deformation is expressed as a percentage of the initial force.

Tensile stress relaxation:

The phenomenon that the tensile force gradually decreases over time after a specimen is subjected to constant tensile deformation under pressure is expressed as a percentage of the initial force.

Meets industry standards and regulations:

This ensures that products comply with relevant industry standards and regulations, reducing risks and improving market compliance.

The advantage of a stress relaxation and creep testing machine lies in providing a platform that simulates real-world application environments, enabling researchers to gain a deeper understanding of the long-term stability and deformation behavior of materials, which is crucial for the reliability and durability of products and structures.

If you have any further questions or needs regarding stress relaxation and creep testing machines or other related equipment, please feel free to contact us.
We are dedicated to providing you with professional support and solutions.

 

Feature

Touch interface

With an intuitive and easy-to-use touchscreen interface, users can easily set test parameters and control the machine, improving ease of operation.

Wide temperature range

It has excellent temperature control capabilities and can be tested in a wide temperature range from -70℃ to 250℃.

Precise force measurement system

Employing a high-precision force measurement system, it can continuously measure compressive or tensile forces throughout the entire testing process, accurately measuring the stress relaxation and creep behavior of rubber materials.

Diverse test modes

It supports multiple test modes, including stress relaxation, creep, dynamic and static tests, and allows you to select the appropriate test mode to study the mechanical properties of rubber materials as needed.

High efficiency and automation

By adopting advanced control systems and testing software, automated testing and data acquisition can be achieved, which greatly improves the efficiency and accuracy of testing, while also reducing the possibility of human error.

Good scalability

The testing machine is designed flexibly and can be customized and expanded as needed. For example, additional accessories can be added to support specific testing requirements.

 

Specification

Temperature range
(select one)
-70℃ to 0℃
0℃ to 150℃
Ambient temp+10℃ to 250℃
Temperature display resolution 0.1℃
Temperature accuracy ≤0℃: ±2.0℃
≤100℃: ±1.0℃
≤250℃: ±2.5℃
Test station 3 or 6 stations (select one)   
Load cell capacity 2kN, 5kN, 10kN (select one for each station)
Load accuracy ≤±0.5%
Stroke sensor Magnetic linear encoder
Stroke range 0.001mm to 50.000mm
Stroke accuracy ≤±0.01mm
Speed ​​range 0.1 mm/min to 50 mm/min
Return speed range 0.1 mm/min to 100 mm/min
Speed ​​accuracy ≤±0.5%
Motor AC servo motor
Interior dimensions
(3-station model)
50×50×60cm (W×D×H)
Exterior dimensions
(3-station model)
108×109×193cm (W×D×H)
Power 1∮ AC 220V 50Hz /60Hz (or specify)